dc.description.abstract We report measurements of the ΔG effect and magnetomechanical damping in as-quenched and annealed amorphous wires of Co72.5Si12.5B15 having a saturation magnetostriction λs of about -3 × 10-6. Samples were measured in the as-quenched state, and after annealing at 450°C for times between 30 s and 1000 min. ΔG of up to 10% and magnetomechanical damping up to 0.004 have been found.
dc.source Journal of Magnetism and Magnetic Materials
dc.title Magnetoelastic properties of annealed Co72.5Si12.5B15 amorphous wires


Files in this item

Files Size Format View

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record