SARIKAYA, M2024-08-042024-08-0419950301-7516https://doi.org/10.1016/0301-7516(94)00046-3https://hdl.handle.net/11616/93013The effects of oxidation on flotation recovery of oxidation at 20 degrees C, 50 degrees C and 100 degrees C for periods up to 100 hours were investigated using an alcohol type frother. The recovery of the floated coal decreased from 95 percent to 24 percent after oxidation. As a result of measurements with a low-ash bituminous coal, flotation is suggested as a method of investigating the initial stages of oxidation of coal particles.eninfo:eu-repo/semantics/closedAccess[No Keywords]FLOTATION TEST AS A METHOD FOR STUDYING COAL WEATHERINGArticle431-2313510.1016/0301-7516(94)00046-32-s2.0-0029167122N/AWOS:A1995RG06100003N/A