Altin, S.Aksan, M. A.Yakinci, M. E.Balci, Y.2024-08-042024-08-0420100925-83881873-4669https://doi.org/10.1016/j.jallcom.2010.04.153https://hdl.handle.net/11616/95074In this study, we have fabricated the superconducting single crystal whiskers using glass-ceramic BiSr-CaCuO material. The crystallization kinetic studies (crystallization activation energy, E-a, and the Avrami parameter, n,) were carried out using DTA data. The oxygen diffusion energy was calculated using TG data. XRD and SEM analysis of the whiskers showed Bi-2212 phase formation and the c-axis orientation. The in-plane resistivity, rho(ab), and the out-of-plane resistivity, rho(c), properties of the whiskers were investigated. The thermoelectric power. S(T), value between 10 and 300 K is found to be positive, indicating that charge carriers in the whiskers are holes. We analyzed the thermoelectric power as a function of temperature with Two band model with linear T-term Linear temperature dependence in the thermal conductivity down to T-c and then a sharp rise just below T-c were obtained. (C) 2010 Elsevier B.V. All rights reserved.eninfo:eu-repo/semantics/closedAccessWhiskersBi-based cupratesThermal properties of glassesTransport properties (electric and thermal conductivity, thermoelectric effects)The single crystal superconducting Bi-2212 whiskers fabrication and their thermal transport propertiesArticle5021162310.1016/j.jallcom.2010.04.1532-s2.0-77954242457Q1WOS:000280066500008Q1