dc.description.abstractThis in vitro study aimed to evaluate the internal and marginal adaptation of crowns produced from partially crystallized and fully crystallized lithium disilicate CAD-CAM blocks using direct view and the silicone replica method. The mandibular first molar was used as an abutment. A total of twenty crowns (n = 10) were produced using milling CAD-CAM. The direct viewing technique was used to measure the marginal gap. The measurement of internal adaptation was conducted using the silicone replica technique. Following the subsequent glazing procedure, all crowns underwent another round of measurements. The paired samples t-test was used to compare two related continuous variables. The study revealed that the mean value of the marginal gap of the partially crystallized block is significantly higher than the fully crystallized block both before and after the glazing process. A statistically significant difference was found before and after glazing of the partially crystallized block in the marginal gap values. The fully crystallized crowns showed better marginal gap values than the partially crystallized ones. No change was observed before and after the glaze in the fully crystallized block. The recommended limit of 120 mu m for the marginal gap of lithium disilicate CAD-CAM crowns was never exceeded.
dc.description.sponsorshipCukurova University Scientific Investigation Project [TSA-2022-15450]
dc.description.sponsorshipThis study was supported by the Cukurova University Scientific Investigation Project (Project number: TSA-2022-15450), Adana, Turkiye.
dc.identifier.doi10.1007/s10266-025-01104-6
dc.identifier.endpage107
dc.identifier.issn1618-1247
dc.identifier.issn1618-1255
dc.identifier.issue1
dc.identifier.orcid0000-0002-7602-8101
dc.identifier.pmid40220251
dc.identifier.scopus2-s2.0-105002354196
dc.identifier.scopusqualityQ1
dc.identifier.startpage101
dc.identifier.urihttps://doi.org/10.1007/s10266-025-01104-6
dc.identifier.urihttps://hdl.handle.net/11616/109874
dc.identifier.volume114
dc.identifier.wosWOS:001465090100001
dc.identifier.wosqualityQ2
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.indekslendigikaynakPubMed
dc.language.isoen
dc.publisherSpringer
dc.relation.ispartofOdontology
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WOS_20250329
dc.subjectMarginal gap
dc.subjectInternal gap
dc.subjectLithium disilicate glass ceramic
dc.subjectSilicone replica technique
dc.titleEvaluation of the marginal and internal gaps of partially crystallized versus fully crystallized lithium disilicate CAD-CAM crowns
dc.typeArticle

Dosyalar