Effect of welding parameters on microstructure and mechanical properties of AA7075/AA5182 alloys joined by TIG and MIG welding methods

dc.authoridÇELİK, Yahya Hışman/0000-0003-1753-7712
dc.authoridçetkin, edip/0000-0002-0217-5897
dc.authoridTEMİZ, ŞEMSETTİN/0000-0002-6737-3720
dc.authorwosidÇELİK, Yahya Hışman/HTP-6058-2023
dc.authorwosidçetkin, edip/ABB-4345-2020
dc.authorwosidTEMİZ, ŞEMSETTİN/ABG-7809-2020
dc.contributor.authorCetkin, Edip
dc.contributor.authorCelik, Yahya Hisman
dc.contributor.authorTemiz, Semsettin
dc.date.accessioned2024-08-04T20:47:02Z
dc.date.available2024-08-04T20:47:02Z
dc.date.issued2020
dc.departmentİnönü Üniversitesien_US
dc.description.abstractIn this study, V and X welding grooves were opened to the forehead positions of the AA5182 and AA7075 aluminum alloy pairs and these alloy pairs were joined with tungsten inert gas ( TIG) and metal inert gas (MIG) methods. Three different welding currents were used in joints. Gas flow rates of 12 and 17 l/min at the TIG welding and wire feed rates of 38 and 45 cm/min at MIG welding were selected. The effect of the welding grooves, welding current, gas flow rate and wire feed rate on microstructure and mechanical properties were investigated. Microstructures of welding zones were analyzed by an optical microscope and a scanning electron microscope (SEM). Vickers hardness of these zones was also measured. In addition, tensile and fatigue tests were carried out. Fracture mechanisms of failed specimens were conducted after the tensile tests were examined by using SEM. The highest hardness, tensile and fatigue strengths were obtained from the alloy pairs joined by opening X welding groove with TIG welding method. These values were 89 HV, 262.87 MPa, and 131.5 MPa, respectively. Similarly, the lowest tensile and fatigue strengths were obtained from the alloy pairs joined by opening V welding groove in the TIG welding method. These values were, respectively, 94.48 MPa and 19.1 MPa. However, the minimum hardness value was measured as 58 HV from the alloy pairs joined by opening V welding groove with MIG welding methods. In addition, it was observed on the fracture surfaces that the grain distributions and mechanisms differed depending on the welding methods, welding groove, and welding parameters.en_US
dc.description.sponsorshipBatman University; Batman University Scientific Research Projects Unit (BTUBAP) [2017-PhD-2]en_US
dc.description.sponsorshipThe authors would like to thank Batman University for the financial support of Batman University Scientific Research Projects Unit (BTUBAP) under the project of 2017-PhD-2.en_US
dc.identifier.doi10.1007/s40430-019-2119-7
dc.identifier.issn1678-5878
dc.identifier.issn1806-3691
dc.identifier.issue1en_US
dc.identifier.scopus2-s2.0-85076413854en_US
dc.identifier.scopusqualityQ2en_US
dc.identifier.urihttps://doi.org/10.1007/s40430-019-2119-7
dc.identifier.urihttps://hdl.handle.net/11616/99100
dc.identifier.volume42en_US
dc.identifier.wosWOS:000521968700001en_US
dc.identifier.wosqualityQ2en_US
dc.indekslendigikaynakWeb of Scienceen_US
dc.indekslendigikaynakScopusen_US
dc.language.isoenen_US
dc.publisherSpringer Heidelbergen_US
dc.relation.ispartofJournal of The Brazilian Society of Mechanical Sciences and Engineeringen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectAluminum alloysen_US
dc.subjectFatigue strengthen_US
dc.subjectMicrohardnessen_US
dc.subjectMicrostructureen_US
dc.subjectTensile strengthen_US
dc.titleEffect of welding parameters on microstructure and mechanical properties of AA7075/AA5182 alloys joined by TIG and MIG welding methodsen_US
dc.typeArticleen_US

Dosyalar