Effect of Different Acid Treatments on the Shear Bond Strength of Computer-Aided Design and Manufacturing (CAD-CAM) Ceramics for Dental Applications
dc.authorwosid | yildirim avcu, guler/K-2278-2017 | |
dc.contributor.author | Yildirim, G. | |
dc.date.accessioned | 2024-08-04T20:45:52Z | |
dc.date.available | 2024-08-04T20:45:52Z | |
dc.date.issued | 2018 | |
dc.department | İnönü Üniversitesi | en_US |
dc.description.abstract | The purpose of this in vitro study was to compare the shear bond strengths (SBS) of hybrid ceramic; Vita Enamic (VE), zirconia-reinforced lithium silicate ceramic; Vita Suprinity (VS), feldspathic ceramic; Vita TriLuxe forte (VT), and lithium disilicate ceramic; IPS e.max CAD (IPS). Eighty specimens were prepared from four different CAD-CAD ceramic materials. The CAD-CAM ceramic specimens were randomly divided into two subgroups according to acid types: phosphoric (P) acid and hydrofluoric (HF) acid. Resin cement (Panavia V5; Kuraray, Japan) was applied using a 3 x 3-millimeter mold. All specimens were stored in distilled water at 37 degrees C for 24 hours. The SBS test was performed using a universal testing machine (0.5 mm/min). Two-way ANOVA was used to detect significant differences among the CAD-CAM ceramic materials and acid types. Subgroup analyses were conducted using Tukey HSD post-hoc test (p < 0.05). The lowest SBS value was seen in the VE group (4.5 +/- 2.2 MPa) for P acid etching. The highest SBS value was seen in the IPS group (19.5 +/- 8.3 MPa) for HF acid etching. | en_US |
dc.identifier.doi | 10.4416/JCST2018-00031 | |
dc.identifier.endpage | 395 | en_US |
dc.identifier.issn | 2190-9385 | |
dc.identifier.issue | 4 | en_US |
dc.identifier.scopus | 2-s2.0-85064212901 | en_US |
dc.identifier.scopusquality | Q4 | en_US |
dc.identifier.startpage | 391 | en_US |
dc.identifier.uri | https://doi.org/10.4416/JCST2018-00031 | |
dc.identifier.uri | https://hdl.handle.net/11616/98754 | |
dc.identifier.volume | 9 | en_US |
dc.identifier.wos | WOS:000454957800004 | en_US |
dc.identifier.wosquality | Q3 | en_US |
dc.indekslendigikaynak | Web of Science | en_US |
dc.indekslendigikaynak | Scopus | en_US |
dc.language.iso | en | en_US |
dc.publisher | Goller Verlag Gmbh | en_US |
dc.relation.ispartof | Journal of Ceramic Science and Technology | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.rights | info:eu-repo/semantics/closedAccess | en_US |
dc.subject | Shear bond strength | en_US |
dc.subject | CAD-CAM ceramics | en_US |
dc.subject | resin cement | en_US |
dc.title | Effect of Different Acid Treatments on the Shear Bond Strength of Computer-Aided Design and Manufacturing (CAD-CAM) Ceramics for Dental Applications | en_US |
dc.type | Article | en_US |