Effects of different glass fibers on the transverse strength and elastic modulus of repairing acrylic resin

dc.contributor.authorPolat, Tülin N.
dc.contributor.authorÖzdemir, Derya Doğan
dc.contributor.authorTopucuoğlu, Sedef
dc.contributor.authorGül, Esma Başak
dc.date.accessioned2020-07-09T07:50:30Z
dc.date.available2020-07-09T07:50:30Z
dc.date.issued2013
dc.departmentİnönü Üniversitesien_US
dc.description.abstractÖz (İngilizce): Objectives: The aim of this study was to evaluate the transverse strength and the elastic modulus of a heat- polymerized denture base resin repaired by adding various glass fibers into an autopolymerizing acrylic resin. Background: The key problems frequently encountered in dentures are fractures. A durable repairing system for a denture base fracture is desired to avoid recurrent fracturing. Materials and Methods: Fifty rectangular (65 mm × 10 mm × 2.5 mm) heat polymerized resin specimens were prepared which were divided in to five groups, with each including ten specimens. For the repairing procedure, samples with the autopolymerizing resin reinforced with stick, woven and chopped glass fibers were prepared. In addition, control samples with the autopolymerizing resin alone (in the absence of the glass fibres) were also obtained. Three-point bending tests were performed on all specimens. Results: The mean transverse strength for the control samples was 78.93 MPa. The specimens repaired with stick fiber reinforced resin exhibited the highest mean transverse strength of 83.16 MPa. The mean elastic modulus of the control specimens was 2121.86 MPa. The mean elastic modulus of the stick group was 7420 MPa. The elastic modulus values of the stick fiber reinforced specimens were significantly higher than the other groups (p < .05). Conclusions: Amongst all samples, the transverse strength and elastic modulus of the stick fiber reinforced samples was found to be the highest.en_US
dc.identifier.citationTülin N. P., DERYA ÖZDEMİR D., Sedef T., ESMA BAŞAK GÜL A. (2013). Effects of different glass fibers on the transverse strength and elastic modulus of repairing acrylic resin, Cumhuriyet Dental Journal, İnönü Üniversitesi, Malatya.en_US
dc.identifier.endpage173en_US
dc.identifier.issn1302-5805
dc.identifier.issn2146-2852
dc.identifier.issue3en_US
dc.identifier.scopus2-s2.0-84885093021en_US
dc.identifier.scopusqualityN/Aen_US
dc.identifier.startpage165en_US
dc.identifier.trdizinid175968en_US
dc.identifier.urihttps://hdl.handle.net/11616/16662
dc.identifier.urihttps://search.trdizin.gov.tr/yayin/detay/175968
dc.identifier.volume16en_US
dc.indekslendigikaynakTR-Dizinen_US
dc.indekslendigikaynakScopusen_US
dc.language.isotren_US
dc.publisherCumhuriyet Dental Journalen_US
dc.relation.ispartofCumhuriyet Dental Journalen_US
dc.relation.publicationcategoryMakale - Ulusal Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectDiş Hekimliğien_US
dc.titleEffects of different glass fibers on the transverse strength and elastic modulus of repairing acrylic resinen_US
dc.typeArticleen_US

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
Küçük Resim Yok
İsim:
Yeni Microsoft Word Belgesi.docx
Boyut:
21.73 KB
Biçim:
Microsoft Word XML
Açıklama:
Makale Dosyası
Lisans paketi
Listeleniyor 1 - 1 / 1
Küçük Resim Yok
İsim:
license.txt
Boyut:
1.71 KB
Biçim:
Item-specific license agreed upon to submission
Açıklama: